Abstract
Effects of B content and heat treatment on properties of gas atomized powders with Ni-10mass%Cr-36mass%Mo-Xmass%B compositions (X=1.5∼4) were investigated. Examined powders were produced by gas atomization, followed by sieving under 150 μm. These powders were heat treated at various temperatures to investigate the effect of heat treatment temperature.As a result, tetragonal M3B2, tetragonal M5B3 and orthorhombic M3B2 type complex borides were observed in examined powders before and after the heat treatment. Compositions and crystal structures of complex borides varied depending on B contents in examined powders, hereby compositions of Ni-based matrix phases also varied. Vickers hardness after the heat treatment at 1473 K increased with increasing B content.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Japan Society of Powder and Powder Metallurgy
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.