Three Pultruded Fibre Reinforced Polymer (PFRP) 152 x 152 x 6.4mm Wide Flange (WF) beams were fabricated with a central two-plate splice joint. The 6.4mm thick PFRP splice plates were 210, 410 and 610mm long. Each beam was tested in symmetric four-point bending about its major and minor-axis and deflections, rotations and surface strains were recorded. Beam transverse stiffnesses, support rotations and splice rotational stiffnesses were quantified and compared with theoretical predictions. Predicted deflections were 3.5% to 18.5% larger and support rotations were 10% smaller to 14.2% larger than the experimental values. Splice end rotations were generally poorly predicted.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.