Siberian larch (Larix sibirica Ledeb.) timber is suitable for many uses in the mechanical wood industry. Drying it without any decrease in value, however, is difficult and slow. The purpose of this research was to compare the drying quality of Siberian larch timber dried with three different conventional schedules taking into account the density and annual growth of wood. Five drying tests were performed. The final moisture content (MC), MC gradient, cracks, deformations (bow, crook, twist and cup) and case hardening were measured from the dried timber. The basic density particularly affected the MC, as shown in the differences regarding dried wood, with the denser wood having higher final MC and MC gradient. It was also found that large annual growth increased some deformations. Most of the measured factors were best after drying at the highest temperatures used; however, a slightly different trend was observed for bow, twist and cup. MC factors and twisting were the most problematic properties in drying according to this study. Sorting Siberian larch timber, particularly according to density, would improve the MC properties of dried timber by ensuring sufficient drying time, as economically as possible, for each timber piece.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.