We have investigated the interfacial control effects of the atomic layer deposition (ALD)-Al2O3 on the crystalline and electronic characteristics of LaAlO3/Ge metal–oxide–semiconductor (MOS) structures. X-ray photoelectron spectroscopic analysis revealed that Al2O3/Ge interfaces are much more stable than LaAlO3/Ge and La2O3/Ge interfaces for the formation of Ge oxides owing to the interfacial reaction. For the LaAlO3/ALD-Al2O3/Ge structure, Al2O3 interfacial layers with thicknesses less than 1 nm effectively suppress the interfacial reaction between LaAlO3 and Ge. The thickness of Ge oxides formed at the ALD-Al2O3/Ge interface decreases with increasing Al2O3 thickness and the stack structure is thermally stable against postdeposition annealing at 600 °C. These results indicate that interfacial reaction mainly arises during the sputtering-LaAlO3 deposition, not the ALD-Al2O3 deposition. On the other hand, capacitance equivalent oxide thickness decreases with increasing interfacial ALD-Al2O3 thickness, because the formation of Ge oxides at the interface is effectively suppressed by ALD-Al2O3 interfacial layers. It can be concluded that ALD-Al2O3 is promising as an interfacial control layer between Ge substrates and high-k dielectrics.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.