Abstract

We present a systematic analysis of the iron loss behavior of grain oriented silicon steels containing different Si contents using transmission electron microscopy. When the silicon content changed in the range of 3–6.5 wt%, the iron loss showed a convex profile and the maximum iron loss was observed in 5.2 wt% silicon steel. This maximum iron loss should be ascribed to the formation of antiphase boundaries that acted as pinning centers in the magnetic domain wall.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.