In this article, we investigate the deposition and characterization of oxide layer grown by using the trisilylamine (N(SiH3)3, TSA)-based as the precursor. The deposited silazane-based oxide film was converted as the SiO2 film by optimizing the conditions of ultraviolet curing, steaming, and high temperature annealing in N2 ambient, even with high pressure conditions. The optimum conditions consist of 650 °C steaming and 1100 °C annealing temperature in N2 ambient. In addition, the film stress can be significantly reduced at high pressure and low temperature annealing (<400 °C).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.