Abstract
Temperature and humidity are the main factors that cause the decomposition of Nomex paper widely used as turn-to-turn insulation material of mining dry-type transformers. In this study, for understanding the effect of ambient humidity and thermal aging on the properties of Nomex paper, specimens with the initial moisture content of 7% were aged in the oven for 168, 504, 672 h at 180°C, respectively. After thermal aging, corona discharge experiments of unaged and aged specimens with different aging degrees were carried out at different relative humidity (RH) levels from 10 to 70%. The characteristic parameters of corona discharge, such as the average discharge amplitude and the number of discharges, were measured. Then, the surface conductivity and the surface potential decay rate were measured. The morphology and attenuated total internal reflectance Fourier transform infrared spectroscopy were also analysed for explaining the difference of properties between unaged and aged specimens. The experiment results indicate that the average discharge amplitude decreases with the increase of RH or the deepening of the aging degree of specimens, but the number of discharges shows the reversal tendency. The changes in the physical structure and chemical composition, which is induced by the hydrolysis reaction of Nomex paper, accelerate the surface potential decay and increase the surface conductivity.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.