The purpose of this study is to investigate the effects on the aluminium alloy plate AL 6061 of triggering fluxes and solder parameters and depth to width ratio (DWR). The welding process for argon gas tungsten arc (GTA) was conducted on the 6061 plate aluminium alloy without filling metals. The fluxes were activated by SiO2, TiO and Fe2o3. Mixed fluxes were used to analyze the effect on solder penetration. Using the experimental technique of GTA soldering using activated flux, a welding Perl of 10 mm with a single pass soldering aluminium alloy plate has been fully mounted. The study concluded that the TIG soldering of SiO2 and Fe2o3 fluxes led to a substantial increase of welded bead penetration and that 6,061 alloys sold with the highest ratio of depth to width were created by the SiO2 flux.