Abstract

Red oak, sweetgum, and yellow-poplar lumber was machined into 3 by 15 by 150-mm (tangential by radial by longitudinal) miniature beams. Moisture content was determined from a subset for calculating the ovendry weight of test samples prior to treatment. Samples were weighed, water saturated, and subjected to a partial hydrolysis at 150°C for 30 minutes in 1 percent sulfuric acid, water, or 1 percent sodium hydroxide solutions. Untreated controls were also used. The beams were ovendried to a constant weight, and then the modulus of elasticity, density, and mass loss (ML) were determined. Modulus of elasticity values were corrected to eliminate density variation by calculating the specific modulus of elasticity (SM) for property comparisons. The species and treatments interacted to significantly affect SM. Sweetgum produced a lower SM in all treatments, and the water treatment consistently reduced SM. The species and treatment factors acted independently of one another with respect to ML. Sweetgum lost significantly more mass than the other species, likely because of corresponding reductions in holocellulose. An acid treatment produced the greatest ML.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.