Abstract
The purpose of this study is to investigate and compare effect of bracket bonding-debonding by nano-composite and composite adhesives on mechanical properties of tooth enamel. Orthodontic brackets were bonded to the enamel surface and the mechanical properties of tooth enamel were studied by nano-indentation technique after bracket removal. Twenty human premolar teeth were prepared and divided into two groups. In one group, orthodontic brackets were bonded by a conventional composite adhesive and in the other group a dental nano-composite was used for bonding the brackets on the buccal surface of tooth enamel. The brackets were then debonded with a sharp-edged debonding pliers. After debonding the brackets, the teeth were sectioned transverse to their longitudinal axes from the middle of the bracket bonded regions. Nano-indentation experiments were performed on the enamel section at two regions: intact enamel and under-the-bracket enamel. Then mechanical properties of the enamel at these two regions, including elasticity modulus, hardness and fracture toughness were determined from the nano-indentation test results for both types of adhesives. Using the nano-composite decreases the magnitudes of elasticity modulus and hardness of the dental enamel under the brackets significantly in comparison with the conventional orthodontic adhesives. However, no significant difference is seen between the fracture toughness reductions due to the use of composite and nano-composite adhesives.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have