The present studies are to investigate the microstructure features and macroscopical hardness during transformation from austenite to pearlite without and with 12T magnetic field on Fe-1.1%C alloy. It is found that 12T magnetic field can increase the area fraction of abnormal microstructure and the average width of secondary cementite in Fe-1.1%C alloy by remarkably decreasing the Gibbs energy needed for the ferrite transformation. The macroscopical hardness of the specimens heated with 12Tmagnetic field is lower than the specimens without magnetic field. The reason is that the magnetric field increase the lamellar spacing of pearlite