The effect of introduction of 0.5 – 2 mol.% Yb2O3 additional doping oxide into ZrO2 – 10 mol.% Sc2O3 solid solutions on the phase composition, structure and electrophysical properties has been studied. ZrO2 stabilization due to the joint effect of 10 mol.% Sc2O3 and 2 mol.% Yb2O3 provides for the formation of transparent homogeneous crystals with a cubic structure having high phase stability. Mechanical grinding of the crystals has not changed their phase composition, the powders retaining the initial fluorite crystalline structure. We show that the high-temperature electrical conductivity of the crystals decreases with an increase in the Yb2O3 concentration.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.