Abstract

High titania slag has become a good raw material in the development of titanium. Ilmenite is reduced first and then smelted in an electric arc furnace to separate iron from the high titania slag. Therefore, enhanced reduction of ilmenite concentrate can reduce smelting time and energy consumption. Wet grinding method, which is often used to reduce particle size and improve the balling ability of ilmenite, was proposed to enhance the reduction. The effect of wet grinding on the carbothermic reduction of ilmenite was investigated. The wet grinding treatment was found to result in a high reduction rate and improve metallisation. The metallisation degree of reduced ilmenite concentrate increased as the time of wet grinding increased. Under the constant reduction conditions, the degree of metallisation improved from 68.58% to 87.32% while the FeO content decreased from 10.62 to 5.28% as the wet grinding time increased from 10 to 60min.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.