Abstract
To refine and spheroidize the microstructures of hypereutectic Al-Si-Fe alloys, a novel method of wavelike sloping plate (WSP) rheocasting was proposed, and the effect of the WSP rheocasting on the microstructures of hypereutectic Al-18 pct Si-5 pct Fe alloys was investigated. The results reveal that the morphologies of the primary Si crystal, the Al18Si10Fe5, and the Al8Si2Fe phases can be improved by the WSP rheocasting, and various phases tend to be refined and spheroidized with the decrease of the casting temperature. The alloy ingots with excellent microstructures can be obtained when the casting temperature is between 943 K and 953 K (670 °C and 680 °C). During the WSP rheocasting, the crystal nucleus multiplication, inhibited grain growth, and dendrite break-up take place simultaneously, which leads to grain refinement of the alloys.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.