Abstract
To evaluate the microshear bond strength of resin cements to yttrium-stabilized tetragonal zirconium oxide surfaces after water storage for 24 h or 1 year. Four self-adhesive (BisCem, G-Cem, RelyX Unicem, SeT) and one conventional resin cement (RelyX ARC) were tested. The materials were mixed and inserted in tubes (0.75 mm diameter × 1 mm height) that were placed over the zirconium oxide surface. Specimens were tested after 24-h or 1-year water storage. Microshear testing was performed using a universal testing machine. Shear bond strength results were analyzed using two-way ANOVA and Tukey's test (5%). After 24-h water storage, no difference was found between G-Cem and RelyX Unicem resin cements; however, their bond strength means to zirconium oxide were statistically higher than RelyX ARC. The bond strength values of all resin cements dropped significantly after 1 year of water storage. G-Cem presented the highest values among cements after long-term water exposure. One-year water storage decreased the microshear bond strengths to zirconium oxide for all resin cements tested.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.