Abstract

PurposeThe aim of the present study is to evaluate the effect of water contamination on the shear bond strength (SBS) and adhesive remnant index (ARI) score of self-ligating brackets. Materials and methodsOne conventional bracket and three different self-ligating brackets were bonded onto 160 bovine permanent mandibular incisors, divided randomly into 8 groups. For each type of bracket, 20 samples were bonded on dry enamel and 20 after water contamination. After 24h, all specimens were tested for SBS using an Instron Universal Testing Machine, and ARI scores were evaluated. ResultsAll groups showed clinically adequate SBSs. Quick brackets bonded onto dry enamel showed significantly higher SBSs than all other groups tested, whereas the lowest shear strength values were recorded for Step, Quick, and Damon 3MX brackets bonded onto contaminated enamel and for Damon 3MX onto dry enamel. Frequency distribution of ARI Scores showed a prevalence of ARI “2” and “3” for all the groups tested. ConclusionsWater contamination reduces the SBS of self-ligating brackets, but significant differences have been found only for Quick brackets. All groups showed a significant higher frequency of ARI Score of “2” and “3”.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.