Abstract

The effect of water in the reactant gas on the catalytic activity for CO oxidation over Au/Co3O4 catalysts has been investigated. Water in the reactant gas had a negative effect on the catalytic activity for CO oxidation in Au/Co3O4 catalyst. Furthermore, it was observed that the average particle size of gold on Au/Co3O4 catalysts increased after stability testing both in dry and wet conditions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.