Abstract
(Ti1-xWx)C solid solutions (x = 0.05, 0.15, 0.25, 0.35) were synthesized by carbothermal reduction and then were used as hard phases to prepare (Ti,W)C-Ni3Al cermets by vacuum sintering. (Ti,W)C-Ni3Al cermets showed weak core-rim structure carbide particles embedded in Ni3Al binder. As W content in (Ti,W)C increased, core-rim structure of carbide particles got weaker and the contrast of particles lowered down in SEM-BSE morphologies. Furthermore, the densification of cermets was promoted with W content in solid solution increasing, meanwhile TRS and toughness of cermets were improved obviously. In this paper, the wettability of molten metal on different group transition metal carbides was discussed in detail based on valence-electron configurations (VECs) of carbides.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.