Abstract

The current study examines how the self-lubricating characteristics of the novel TiSiVN coating affect the chip formation process and chip sliding velocity during the dry turning of Ti6Al4V titanium alloy. The serration bands tend to straighten at a cutting speed of 125 m/min, which is the main cause of the chips being straightened without tangling for both coated tools. TiSiVN coated tool accounts for higher chip sliding velocity due to the generation of lubricious phases, whereas the higher VS for uncoated tool indicates high tool wear at the highest cutting speed of 125 m/min. Further, r and θn tend to have an inverse relationship with VS, with 125 m/min cutting speed remaining an exception due to severe changes in tool wear dynamics. The reduction of friction helped to lower the localized strain along the shear bands and the effective stress at the beginning of the formation of the serrated tooth.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.