Abstract

This study uses a nanofibrous membrane produced using electrospinning to undergo processing, to form a yarn with twist of 2.4, 4.0, 5.6, and 7.2 thermal pulsed currents (twist/cm). The optimum twist multiplier values are chosen and used to discuss the tendency of stress and strain. Furthermore, the draw ratios of 1.1, 1.2, 1.3, and 1.4 are applied, to determine which provides an optimum strength. The result showed that yarn with fineness of 40tex corresponding with twist multiplier of 36 and draw ratio of 1.4 have strength of 219.3 g (stress of 5.14 cN/tex). This result can be applied for the further study of continuous nanofibrous yarn.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.