Abstract

The effectiveness and safety of the mouthguard are greatly affected by its thickness. The aim of this study was to investigate the effect of thermal shrinkage of the extruded sheet on the mouthguard thickness depending on the amount of undercut of the model. Mouthguard sheet was used a 4.0 mm thick ethylene-vinyl acetate resin manufactured by extrusion molding. The sheets were placed in the vacuum forming machine with the sheet extrusion direction either vertical (condition V) or parallel (condition P) to the model’s centerline. The working models were three hard plaster models trimmed so that the angles of the anterior teeth to the model base were 90?, 100?, and 110? (Models A, B, and C). The sheet was softened until it sagged 15 mm, and then suction was continued for 30 s. Measurement points of the mouthguard were the incisal portion (incisal edge and labial surface) and molar portion (cusp and buccal surface). The differences in the reduction rate of the thickness due to model form and extrusion direction were analyzed using two-way ANOVA and Bonferroni’s multiple comparison tests. Differences in thickness depending on the extrusion direction of the sheet were observed in Models B and C on the labial surface and in all models on the buccal surface, and the thicknesses obtained under condition P were significantly thinner than those obtained under condition V. The thicknesses of the incisal edge and the cusp were not affected by the extrusion direction. The result of this study was suggested that the labial and buccal thickness of the mouthguard was secured by placing the sheet in the extrusion direction vertical to the model’s centerline. Furthermore, it was clarified that the presence of the undercut of the model tends to increase the influence of the extrusion direction of the sheet on the thickness of the mouthguard.

Highlights

  • The effectiveness and safety of mouthguards depend on the material and thickness of the sheet [1] [2] [3]

  • The aim of this study was to investigate the effect of thermal shrinkage of the extruded sheet on the mouthguard thickness depending on the amount of undercut of the model

  • Differences in thickness depending on the extrusion direction of the sheet were observed in Models B and C on the labial surface and in all models on the buccal surface, and the thicknesses obtained under condition P were significantly thinner than those obtained under condition V

Read more

Summary

Introduction

The effectiveness and safety of mouthguards depend on the material and thickness of the sheet [1] [2] [3]. To counter the stress and strain generated during impacts, it is necessary to provide a sufficient thickness of 3 - 4 mm on the labial and buccal sides of the mouthguard [4] [5]. For single-sheet mouthguards, a 4.0mm-thick sheet is often used. Laminated mouthguards reliably provide a suitable thickness, but they may not be readily available to users due to the cost and fabricating time. Various fabrication methods have been investigated to secure the thickness after formation with a single sheet [6] [7] [8]

Objectives
Methods
Results
Conclusion