Abstract
Tungsten- and nickel-containing coatings have been produced on the surface of synthetic diamond crystals by rotary chemical vapor deposition (RCVD) using tungsten hexacarbonyl, W(CO)6, and nickelocene, Ni(C5H5)2, as gaseous precursors. The thickness, composition, and morphology of the coatings have been shown to depend on the RCVD process duration and reactant concentrations in the vapor phase. The synthetic diamond microcrystals with tungsten- and nickel-containing coatings have been used to produce copper–diamond heat-conducting composites. Powder mixtures containing 50 vol % diamond with a particle size of 50, 100, or 200 μm have been consolidated by spark plasma sintering or hot pressing. It has been shown that the highest relative density (97%) and thermal conductivity (340 W/(m K)) are offered by the composites produced by spark plasma sintering using tungsten carbide-coated 50-μm diamond crystals.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.