Abstract
Glasses of the following composition were prepared: (2.5-x)CaO.x/3La2O3.2SiO2 (0 < or = x < or = 1). Their behavior when soaked in a simulated body fluid (SBF) was studied by means of electron microscopy (EM) equipped with an energy-dispersive system (EDS) for elemental analysis, IR spectroscopy, and x-ray diffraction. All the studied glasses react with SBF by forming a calcium phosphate layer. This layer appears to be increasingly thinner with increasing amounts of La2O3 substituted. The experimental results are in good agreement with mechanisms reported in the literature. Moreover they suggest that lanthanum oxide is retained in the layer below the phosphate. After 6 days of soaking, crystalline hydroxyapatite is formed in the case of La2O3 free glass.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.