Abstract
This article presents the bending strength and flexural properties of the glued T-type spruce loose tenon construction joints with and without reinforced plastic clamp fitting. Construction joints are designed according to Eurocode 5. The samples are made from European spruce (Picea abies Karst.) C24 class construction material with relative wood moisture 18% and relative wood density 410 kg/m3. Samples are assembled with water/high temperature resistant polyurethane adhesive and polyvinyl acetate dispersion adhesive. The total number of samples is 48. The sample width is 95mm and thickness is 45mm. Samples were subjected to moisture, weight controls and 48h stored in the climate chamber before practical bending load test. T-type loose tenon joint construction samples with reinforced plastic clamp fittings glued with polyurethane adhesive under bending load are 2.6% stronger and 13.8% less flexural then without reinforced plastic clamp fittings. T-type loose tenon joint construction samples with reinforced plastic clamp fittings glued with polyvinyl acetate dispersion adhesive under bending load are 9.7% weaker and 20% less flexural then without reinforced plastic clamp fittings. The accuracy of the developed bending strength, deformability and elasticity modulus of the examined construction joints was verified positively by experimental studies.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.