It was found that cooling treatment during the presintering process had considerable influence on the initial permeability of Mn 0.516Zn 0.395Fe 2.089O 4 ferrite. The initial permeability increased to a large extent for the samples obtained from quenched powders. This phenomenon was not connected with the microstructure of the Mn-Zn ferrite.