Abstract

Ceramic oxide coatings were produced on pure titanium by plasma electrolytic oxidation in different electrolytes. The variation of coating thickness with applied voltages revealed coating almost kept a steady-state growth rate in electrolyte A and B, but not for electrolyte C. Numerous nodules occurred on the surface of the coatings at 200V in electrolyte A and B, and then nodules disappeared with the applied voltage increasing to 300V. There was no nodules occurred, and pore size was evidently different in electrolyte C. When the applied voltage was 300V, the coating formed in electrolyte C exhibited the highest corrosion potential and lowest corrosion current density in 3.5% NaCl aqueous solution.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.