Abstract

Abstract During the extrusion of magnesium alloys, temperature change could have a significant effect on the outcome. When this effect is not considered, some commonly known defects might be observed, such as hot cracking. In this study, all samples consist of extruded AZ31 and AM50 magnesium alloys as a solid profile, but the methods by which they are cooled, such as air cooling and water quenching, vary. The effects of cooling methods on tensile-compression behavior and the microstructural properties of the samples were investigated. Test samples were obtained in extrusion direction and perpendicular to the extrusion direction separately for mechanical tests. The main purpose of this study was to investigate the effect of different cooling methods on the mechanical properties and microstructural behavior of AZ31 and AM50 magnesium alloys after extrusion, once different cooling methods were applied. According to the microstructural investigation results, an AM50 magnesium alloy has a finer grain structure as compared with an AZ31 alloy according to both cooling methods in the extrusion process. The average grain size values of both alloys were found to be higher for water cooling. Cooling methods have significant effects on the tensile properties of both alloys, depending on their extrusion directions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.