In the past decades, metakaolin additives synthesized by the calcination of kaolin clays have been implemented in cement systems. Their scarcity and high cost promotes the studies on the effectiveness of thermally activated additives of common polymineral clays. This article presents the results of research on the effect of thermally activated heavy loam additives to Portland cement. It was shown that additives of 5–15% heavy loam calcined at certain temperatures in the range of 400—600°C and ground to a certain specific surface area of up to 250–500 m2/kg lead to a more significant increase in the strength, density, and water resistance of cement stone than corresponding metakaolin additives with the specific surface area of 1200 m2/kg.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.