Abstract
The use of rattan and bamboo fibers increases the compressive strength, tensile strength and improves the ductility of concrete. Shell ash also contains pozzolanic compounds that can improve the properties of concrete. In this study, rattan and bamboo were used as concrete fibers and seashell ash was used as filler. The purpose of this study is to measure the compressive and tensile strength of concrete. In this study, rattan and bamboo fibers were added to the concrete mix with a mix design 25MPa. The additive variation is 0%, 0.5%, 1%, 1.5%, 2%. The results showed that the average compressive strength at 28 days was 0.26.29 MPa, 0.5, 19.71 MPa, 1.21.69 MPa, 1.5, 24.72 MPa and 2.18 MPa. Accordingly, the average tensile strength after 28 days was 0.736 MPa, 2,359 MPa, 2,312 MPa, 2.453 MPa and 2,595 MPa. These results show that the addition of rattan and bamboo fibers to concrete can increase the crack resistance of concrete, while the optimal increase in compressive strength with the addition of rattan fiber is achieved only with the change of 1.5%. This indicates that the addition of 1.5% natural fibers improves the tensile strength of concrete.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Similar Papers
More From: E3S Web of Conferences
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.