n-Type (Bi 2Te 3) 0.93(Bi 2Se 3) 0.07 thermoelectric materials doped with various content of TeI 4 (0, 0.05, 0.10, 0.13, and 0.15 wt.%) have been fabricated through the zone melting method. Electrical conductivity ( σ), Seebeck coefficient ( α) and thermal conductivity ( κ) were measured along the crystal growth direction in the temperature range of 300–500 K. The influence of the variations of TeI 4 content on thermoelectric properties was studied. The undoped (Bi 2Te 3) 0.93(Bi 2Se 3) 0.07 exhibited p-type conduction and it translated to n-type when TeI 4 was doped. The increase of TeI 4 content increased the carrier concentration and thus resulted in an increase of σ and a decrease of | α|. The maximum figure of merit ZT (ZT = α 2 σT/ κ) of the zone-melted crystals in the direction parallel to the growth direction showed a value of 0.90 for the sample containing 0.10 wt.% TeI 4.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.