Abstract

The thermal oxidation kinetics of natural rubber containing hydrazine dihydrochloride or hydrazine sulfate used as tackifier were studied, and the effective storage time of natural rubber containing tackifier was predicted with a method of heat accelerated storage aging. The results show that the thermal oxidation activation energy of natural rubber containing hydrazine dihydrochloride is 105.6kJ/ mol, being a little higher than that (104.7 kJ/ mol) of the control. The thermal oxidation activation energy of natural rubber containing hydrazine sulfate is 103.1kJ/ mol, being a little lower than that of the control. The effective storage time of natural rubber containing hydrazine dihydrochloride is 13.4 years at 30°C,27.0years at 25°C, and 55.9years at 20°C. The effective storage time of natural rubber containing hydrazine sulfate is 11.6years at 30°C,23.0 at 25°C, and 46.8years at 20°C.The effective storage times of natural rubber containing two tackifiers hydrazine dihydrochloride or hydrazine sulfate are higher than that of the control at the same condition.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.