Abstract

This work presents the synthesis of CuO-NiO nanocomposites under different synthesis conditions. Nanocomposites were synthesized by merging a green synthesis process with a microwave-assisted hydrothermal method. The synthesis conditions were as follows: concentration of the metal precursors (0.05, 0.1, and 0.2 M), pH (9, 10, and 11), synthesis temperature (150 °C, 200 °C, and 250 °C), microwave treatment time (15, 30, and 45 min), and extract concentration (20 and 40 mL of 1 g saponin/10 mL water, and 30 mL of 2 g saponin/10 mL water). The phases and crystallite sizes of the calcined nanocomposites were characterized using XRD and band gap via UV-Vis spectroscopy, and their morphologies were investigated using SEM and TEM. The XRD results confirmed the formation of a face-centered cubic phase for nickel oxide, while copper oxide has a monoclinic phase. The calculated crystallite size was in the range of 29–39 nm. The direct band gaps of the samples prepared in this work were in the range of 2.39–3.17 eV.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.