Abstract
Magneto-acoustic emission (MAE) measurements were made on samples of pipeline steel under different AC sweep and DC bias field conditions. The MAE activity was found to be highly sensitive to these magnetizing parameters. With increasing amplitude of flux density of the AC sweep field, the MAE RMS voltage increases initially and finally tends to saturate; with increasing DC bias field flux density the MAE RMS voltage shows a peak, exhibiting maximum MAE activity around the upper steep portion of the B-H hysteresis curve. Pulse height distribution analysis of the MAE waveforms indicates that at low fields, near the steep portion of the hysteresis curve, MAE is dominated by 90 degrees domain wall motion, while at high fields, nearing saturation, an additional mechanism of domain rotation giving rise to MAE is suggested. >
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.