This study evaluated the effect of surrounded shade and specimens` thickness on the color adjustment potential (CAP) of a single-shade composite. The composite Vittra APS Unique was surrounded (dual specimens) or not (simple specimens) by a control composite (shade A1, A2, or A3). Simple specimens of the control composite were also confectioned. Opacity and whiteness index for dentistry (WID) were calculated for simple specimens. Color differences between the simple (ΔE*SIMPLE)/ dual specimens (ΔE*DUAL) and the controls were calculated. CAP was calculated based on the ratio between ΔE* SIMPLE and ΔE* DUAL. The tested composite presented lower opacity (53 to 62% vs. 80 to 93%) and higher WID (≈ 42 vs. 18 to 32) than controls. Irrespective of the specimens' thickness (1.0/ 1.5 mm), the lowest values of ΔE* SIMPLE (11.1/ 10.8) and ΔE*DUAL (7.2/ 6.1) were observed using the surrounding shade A1. The shade A3 yielded higher ΔE*SIMPLE (16.4/ 17.1) and ΔE* DUAL (11.3/ 12.3) than the A2 (ΔE*SIMPLE = 13.4/ 14.6; and ΔE* DUAL = 9.7/ 10.3). The specimen`s thickness significantly affected the CAP (0.35 and 0.44 for 1.0 and 1.5 mm, respectively) only for shade A1, which had the highest CAP values. The shade A3 resulted in higher CAP values (0.31) than A2 (0.27) when 1.0-mm thick specimens were used, but similar values were observed for 1.5 thick specimens (≈ 0.29). In conclusion, both surrounding shade and specimen thickness can affect the CAP of a single-shade resin composite.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.