Abstract

The coercive field and spontaneous polarization have been measured as a function of temperature (-10°C to 22°C) for different thicknesses (about 2 mm to 0.5 mm) of triglycine selenate crystals. The thickness dependent dielectric constant has also been measured at frequencies 1 kHz, 10 kHz and 100 kHz. The coercive field is found to be inversely proportional to the thickness of the sample. The spontaneous polarization has been found to decrease with decreasing thickness and the effect is most pronounced at smaller thicknesses. The results can be explained by assuming a single homogeneous surface layer of low dielectric constant. However, the numerical values of surface layer thickness estimated from the coercive field measurements are two order of magnitude higher than those derived from thickness dependent dielectric constant measurements.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.