Abstract

Model alloys Fe-20Cr and Fe-20Cr-20Ni (wt.%) and these alloys doped with 0.5% Si or 2% Mn were exposed to Ar-20%CO2-20%H2O-(0%, 0.1%, 0.5%, 1.0%)SO2 gas mixtures at 650 °C. Alloys of Fe-20Cr-(2Mn) and Fe-20Cr-20Ni-(0.5Si) underwent breakaway oxidation in sulphur-free gases, forming thick iron-rich oxide scales and internal carbides. SO2 additions promoted the maintenance of protective chromia scale on Fe-20Cr-(2Mn) and Fe-20Cr-20Ni-(0.5Si) alloys, but had no benefit for the already high corrosion resistance of Fe-20Cr-0.5Si and Fe-20Cr-20Ni-2Mn alloys. The role of sulphur in retarding carburization is discussed with reference to its strong adsorption on oxide grain boundaries.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.