Abstract
We have studied the effects of suction air pressure on the structural parameters and mechanical properties of yarn. Changing the amount of suction air pressure improves the fiber extent in yam and yarn appearance. Therefore, photographic and fiber tracing methods are used to evaluate, respectively, yam appearance and fiber extent in the yam. To consider the effect of suction air pressure on yarn diameter, yam tension at the yarn-forming zone and yam diameter are measured simultaneously on a friction spinning machine using various levels of suction air pressure, and then the relationship between them is considered using the cross correlation method. The results show that at high suction air pressure, yarn di ameter, yarn unevenness, and yam irregularity decrease, while fiber extent in the yarn and twist efficiency increase. On the other hand, the value of the correlation coefficient demonstrates that there is a high correlation between variations in yam tension and yarn diameter. The results of yam mechanical property measurements show that at high suction air pressure, yam tenacity increases and yarn elongation decreases. Results are reported from experiments on 100% cotton yams.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.