Abstract

The catalytic efficiency of four kinds of activated carbon catalysts derived from coconut shell (SAC), coal tar pitches (PAC), coal (CAC), and oak wood (WAC) was unprecedentedly evaluated in catalytic wet peroxide oxidation (up to 2000h) for m-cresol wastewater. The physical and chemical characteristics of activated carbon catalysts were determined by scanning electron microscopy, X-ray Fluorescence, Brunauer-Emmett-Teller method, Raman spectroscopy and temperature-programmed desorption. The results indicated that the superiority of activated carbon, especially SAC, in m-cresol degradation was ascribed to the quantity of structural electron-rich active sites, which is proportional to the product of the structural disordered degree and specific surface area, and could improve the efficiency of H2O2 usage to above 95%. Upon modification with iron, the catalytic activity of SAC and PAC could be further improved that enhanced above 90% m-cresol conversion even after 2000h continuous reaction under stoichiometric H2O2 dose. Furthermore, an increase in structural Fe (II) content in catalysts, which was generated from the reversible Fe(III)⇌Fe(II) processes, was noticed after effective long-term CWPO processes by the help of structural electron-rich active sites of activated carbon. The intermediates were identified by gas chromatography-mass spectrometry and then calculated by density functional theory.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.