Abstract

AbstractIn biomineralization, amorphous precursors enable formation of complicated crystal shapes and incorporation of organic and inorganic impurities. In some cases the concentrations of the inorganic impurity atoms greatly exceed the thermodynamical (equilibrium) solubility limits. To shed additional light on this, crystallization experiments with Sr‐rich amorphous calcium carbonate (ACC) are carried out. The Sr‐concentration in ACC, Sr/(Ca+Sr) ≈0.3, is more than 60 times larger than its solubility limit in calcite. Crystallization of ACC is accomplished using two different pathways: i) in a high humidity environment at room temperature, and ii) upon heating at 300 °C. In both cases, X‐ray diffraction measurements revealed the formation of particular crystal phases with an ability to take up substantial amounts of Sr. Crystals formed via the humidity route comprised spatially separated regions of almost pure rhombohedral calcite and orthorhombic aragonite/strontianite solid solution with a Sr/(Ca+Sr) ratio equal nearly 0.5. Crystallization of ACC upon heating resulted in the appearance of a new calcite‐like phase with reduced space symmetry, , instead of for regular calcite. Symmetry reduction in this Sr‐rich ‐phase is due to the rotational disorder of flat carbonate groups about the c‐axis, which is responsible for the enhanced lattice capacity of Sr incorporation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.