Uni-axial tensile test was conducted at room temperature on a weak texture AZ31B magnesium alloy at different strain rate, from 2.8×10-5s-1 to 1.1×10-1s-1. The mechanical behavior was investigated. It was found that as strain rate is increased, flat character of the stress-strain curves can be found and {10-12} tension twinning is responsible for this phenomenon. The sample exhibites a brittle fracture at 1.1×10-1s-1 strain rate while exhibites a ductile fracture character at 2.8×10-5s-1 strain rate.