The microstructure and mechanical properties of friction stir welded Al-5.4Mg-0.2Sc-0.1Zr alloy were studied. Defect-free welds were produced in hot extruded, hot rolled and cold rolled initial conditions. Friction stir welding led to the formation of ultrafine-grained structure in stir zone that contributes to overall strengthening. Coherent Al3(Sc,Zr) dispersoids retain partially during welding process that provides a joint efficiency close to 100% in the hot extruded and hot rolled materials. In the cold-rolled state the joint efficiency was found to be only 64%. The relatively low weld strength of the cold rolled material was attributed to the elimination of strain hardening due to the formation of recrystallized structure. It was shown that full strength weld can be achieved in semi-finished products of Al-Mg-Sc alloys in cold-worked and stabilized states being equal to H323 and H341 tempering by friction stir welding.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.