Abstract

This study aims to investigate the effect of stitch row directions on tensile and flexural bending mechanical properties of composite laminates reinforced by glass-fabric. For the fabrication of stitched laminates, a polyester thread was used to stitch the dry fabric glass in fourth cases (longitudinal stitch 0°, transversal stitch 90°, multi-stitching 0°/90°, and 45°/-45° stitch) with 4 mm stitch spacing. The responses of stitched laminates specimens subject to the tests mentioned were compared to the unstitched laminates and discussed. According to our results, the effect of stitching plays opposite roles on the tensile property by decreasing of about 45% and 36% in tensile strength and longitudinal modulus compared to unstitched specimens, respectively. However, an increasing approximately 11.69% to 20.25% in flexural strength found in samples stitched along 0° and multi-stitching 0°/90°, due to the stitch lines through-thickness by arrests temporally of cracks propagation and the delamination progressively propagate between layers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.