Abstract

ABSTRACT Objective: This study used spectrophotometry to examine how staining beverages affect the color stability of three commercial composite materials (nanohybrid composite (A), bulk fill composite (B), and flowable composite (C)) over time. Materials and Methods: Composite discs were randomly divided into groups. The specimens were kept in coffee, tea, red wine, and cola for 14 days at 37°C in the dark. At baseline, 7 days, and 14 days, spectrophotometers measured color. Calculated and analyzed color differences (E). Results: Staining beverages changed the color of all composites. Composite material A had the best color stability, whereas material C stained beverages the most. Red wine and coffee discolored composites most. Discoloration increased over the 14-day immersion period. Conclusion: Composite materials with better color stability were material A. Red wine and coffee discolored composites most. When choosing restorative materials, dentists should consider composite materials’ color stability for long-lasting, visually acceptable results.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.