The microstructure, tensile properties and wear behavior of as-cast Mg–6Zn–4Si alloy with strontium additions at ambient and elevated temperature were investigated by means of X-ray diffraction (XRD), optical microscopy (OM), scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), standard high temperature tensile testing and a pin-on-disc type apparatus. The results indicated that the grain size of the primary Mg2Si decreased initially and then gradually increased with increasing Sr amount. Meanwhile, the morphology of the primary Mg2Si in the alloys changed from large dendritic to polygonal or fine block, and that of the eutectic Mg2Si phase turned to fine fibre with increasing Sr content. Tensile testing results showed that Sr addition improved the ultimate tensile and elongation of the Mg–6Zn–4Si alloys at both ambient temperature and 150°C. Dry sliding wear tests indicated that the change trend of wear rate was basically coincident with that about the average size of the primary Mg2Si phases. Optimal mechanical properties and wear behavior could be achieved by a Sr addition of 0.5%. An excessive Sr addition resulted in the formation of the needle-like SrMgSi compound, which was detrimental to the tensile properties and wear behavior of the alloys.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.