Abstract

In order to control the optical and electrical properties of the transparent conductive oxide, the radio frequency (RF) sputtering power was changed from 30 to 40, 50, and 60W. To optimize the power condition of the SiInZnO (SIZO) layer, we changed the sputtering power from 30 to 60W, systematically. The chemical properties of the SIZO layer were analyzed using X-ray photoelectron spectroscopy (XPS). XPS proved that this change is dominant in thickness. In order to fabricate the SIZO transparent conducting oxide (TCO) with the optimized power of 50W, the transmittance of 99.1% at 550nm and the figure of merit of 12.4×10-3 Ω -1 were obtained.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.