Abstract

Different concentrations of LiF and Cr 2 O 3 were incorporated in Li, Ba aluminosilicate glass to establish their effects on the crystallization process. The kinetics of phase transformations, the final crystalline phase assemblages and the microstructures formed were found to be dependent on the types and concentration of the nucleant involved. Cr 2 O 3 was found to increase the melting temperature and favor crystallization of β-spodumene ss hexacelsian and traces of monoclinic celsian. It also favors volume crystallization of finer grained microstructure. LiF was found to decrease the melting temperature and favor crystallization of β-spodumene ss and monoclinic celsian. LiF in low concentrations greatly facilitates the crystallization process, the β-eucryptite ss/β-spodumene ss transformation and hexacelsian/monoclinic celsian transformation. It also stimulates surface crystallization with holocrystalline coarse non-uniform textures. The effects of various Cr 2 O 3 concentrations were discussed on the basis of the increased viscosity and separation of Cr 2 O 3 and/or chromium spinel phases. The role of LiF was attributed to the role of fluorine ions in reducing the viscosity of the glasses, consequently facilitating crystallization of the structurally more complex silicate in addition to favoring reaching thermodynamic equilibrium.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.