Abstract
Evolution of the morphology of MC carbides with the change of cooling rate and carbon content in two kinds of nickel-base superalloys, K417G and DD33, has been investigated. The morphology of MC carbides evolves from faceted to script-like with increasing cooling rate. Varying the carbon content from 40 × 10−6 to 320 × 10−6, the morphology of carbides changes from blocky, rod-like into script-like. Scanning electron microscopy observation of deep-etched samples indicates that these carbides evolve from octahedral to dendritic and then into well-developed dendrites accordingly in a three-dimensional manner. The morphology evolution is discussed from the viewpoint of the preferential growth orientation of fcc crystals and the carbide growth rate during directional solidification.