Abstract
The higher the fraction of solid phase in the partly solidified melt during pouring, the poorer the mechanical properties of thixocast components. The solid fraction decreases as the pouring temperature rises. Recommended temperature profiles for the pouring cylinder are shown. The flow characteristics of the partly solidified melt hardly changes as the content of solid matter increases.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Mining and Metallurgy, Section B: Metallurgy
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.