Abstract

Ladle slag affects steel cleanliness at the end of the Ruhrstahl-Hereaeus (RH) and holding process. The relationship between composition of ladle slag, total oxygen (TO) and inclusions was investigated using X-ray fluorescence (XRF), infrared absorption, and SEM + EDS methods. The results indicate that TO in steel at the end of RH increases linearly with increasing FeO content in slag. TO is lower when ωCaO/ωAl2 O3(C/A)=1. 5-2. 0 than that of C/A = 1.0–1.4 under an approximate content of FeO. During the holding process, irregular Al2O3 inclusions are newly generated due to slag reoxidation. Additionally, Al2O3-Tix O inclusions are newly generated in the steel when the content of FeO is higher. By combining experimental and thermodynamic calculation results, it is determined that the slag has a good melting property within the zone of C/A=1.2–1.8 and adsorption capacity of Al2O3 when the content of SiO2 in slag is controlled at 4%–6%. The increase in the C/A ratio and the decrease of FeO content in slag can slow down the reoxidation rate.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.