Calcium phosphate ceramics were substituted with several concentrations of zinc ions (0, 5, 10 and 15 mol%) using precipitation method. The effect of sintering temperature at 900 and 1000°C on zinc substituted calcium phosphate ceramics were observed. By increasing the sintering temperature, XRD peaks for zinc substituted calcium phosphate ceramics changed significantly. At sintering temperature of 900°C, hydroxyapatite phase was the major phase in the calcium phosphates containing 0 and 5 mol% zinc. However, at the sintering temperature of 1000°C, hydroxyapatite phase was partly transformed to another phase which was tricalcium phosphate. FESEM observations at sintering temperature of 1000°C exhibit that the particle size of the samples increased with addition of more zinc ions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.